Nanoindentation is an AFM mode where indentation hardness tests are applied to various samples. Nanoindentation typically uses diamond probes or coated afm tips that are hard enough to withstand the pressures exterted using this technique.
Frequency
Nom: 50KHz
Spring Const.
Nom: 225N/m
Geometry
Rectangular
Tip Radius
40nmMaterial
Stainless Steel
Frequency
Nom: 180KHz
Spring Const.
Nom: 40N/m
Geometry
Rectangular
Tip Radius
10 ± 5nmMaterial
Single Crystal DiamondCoating
Highly conductive single crystal diamondB: Reflective Au
Frequency
Nom: 65KHz
Spring Const.
Nom: 2.8N/m
Geometry
Rectangular
Tip Radius
10 ± 5nm
Frequency
Nom: 65KHz
Spring Const.
Nom: 2.8N/m
Geometry
Rectangular
Tip Radius
<5nm
Frequency
Nom: 50KHz
Spring Const.
Nom: 450N/m
Geometry
Rectangular
Tip Radius
40nmMaterial
Stainless Steel
Frequency
Nom: 180KHz
Spring Const.
Nom: 40N/m
Geometry
Rectangular
Tip Radius
<5nmMaterial
Single Crystal DiamondCoating
Highly conductive single crystal diamondB: Reflective Au
Frequency
Nom: 50KHz
Spring Const.
Nom: 225N/m
Geometry
A Rectangular
Tip Radius
40nmMaterial
Stainless Steel
Frequency
Nom: 50KHz
Spring Const.
Nom: 450N/m
Geometry
Rectangular
Tip Radius
40nmMaterial
Stainless Steel
Frequency
Nom: 50KHz
Spring Const.
Nom: 225N/m
Geometry
Rectangular
Tip Radius
40nmMaterial
Stainless Steel